Uv varnish brightness is not enough?

Number of visits:1232 date:2021-12-26 23:26:06

Abstract:

How to increase brightness?

 The main reason: UV varnish viscosity itself is too small, so that the printing coating is too thin; Excessive dilution of ethanol, toluene and other non-reactive solvents; The gloss of the resin itself is not enough; Paper absorption is too strong; Roller is too thin resulting in too little light transfer oil;


Solution: take the necessary cleaning measures for the printed matter to be glazed; Properly adjust the viscosity of light oil; Deploy the type and amount of gloss additives, can add a small amount of wetting agent; The surface of the printed matter can be wiped with a 2% alkali solution.

 

previous: Without the ...

Next: Without the ...

Category: questions

consulting
phone
scan
go back